Grade designations for sheet metals
Sep 12, 2016· A letter, representing temper, follows the first four digits to indicate if the material is supplied already workhardened (H) or heattreated (T), or annealed (O) at the mill. The annealed condition provides the lowest strength and highest elongation of the alloy.